Well, I had this:
(http://www.radbmx.co.uk/archive/albums/v290/orb200181/P3040001.jpg)
but red is poo, and it is a tad scratched, so into a vat of soda, here is 10 seconds into it:
(http://www.radbmx.co.uk/archive/albums/v290/orb200181/P3040004.jpg)
20 Seconds:
(http://www.radbmx.co.uk/archive/albums/v290/orb200181/P3040005.jpg)
Fish it out and have a looksie:
(http://www.radbmx.co.uk/archive/albums/v290/orb200181/P3040007.jpg)
Couple more seconds for luck:
(http://www.radbmx.co.uk/archive/albums/v290/orb200181/P3040008.jpg)
Rinsed under boiling water and a swift wipe with a Brillo Pad:
(http://www.radbmx.co.uk/archive/albums/v290/orb200181/P3040009.jpg)
Will polish out the scratches and make it bling tomorrow
Oh, for all you caustic virgins, here is what i did:
-Jam jar, 2 table spoons of crystals, add cold water 3/4 to the top and mix it up with a fork.
-Get a baking tray that needs a clean and put the chain ring on in, and tip the caustic soda mix on.
-Cough like fook as you are in the kitchen.
-Tip the whole lot into the sink and tip a boiling kettle over it and then run the taps for a min or 2.
-Done.
-
ace
-
** Not to self **
Indoor caustic fun is not good
cant feckin breathe now :(
-
lol mr health and safety.
-
will this work on painted or powder coated items as ive got a few power discs that have poo paint on them
-
bet that smells paint made of poo :LolLolLolLol:
-
:LolLolLolLol: :LolLolLolLol: :daumenhoch:
-
Caustic will strip paint, but it has to be made VERY strong and it takes forever.
Nitromors is the nuts for paint :)
-
nitromours is pants for powder coating as i have tried for the 5th time to get my gt frame back to bare :-\
Wonder if a good old heat gun will do it ???
-
yeah, heat is good for Powder Nana.
Glass paper works too, but it is a pain in the arse mate, i hate to say it but with powder, take it to get blasted.
-
no chance im a skint flint sweaty sock im not getting anything blasted ;D i will do it myself as usuall ;)
What you want a gt chainring for anyways ??? is it for that dp of yours with the block stem?????
-
because it was cheap :)
-
want to sell it orb? got a nice powerdisc to match that and a gt pro to put it on. :daumenhoch:
-
orb, tricky, we need a caustic thread in the how to section
-
orb with the caustic and the tabs youll be coughing like 90 year old in no time mate lol
-
do you think this would work on some tech 77 levers or will it melt any bits on them?
-
i have done dia compe tech 3s and 45 degree levers and have had no probs
-
cool, how long did you leave them in for or do you just keep an eye on them and take them out often to check if its doing the job.
-
jimbo i need them tech 77's mate for a rider
-
who said i had any, i was just enquiring for a friend of mine :LolLolLolLol:
-
just keep checking should only take a minute or so dont leave them for to long or you will kill them :'(
-
ok nice one, shall have a go at it. :daumenhoch:
-
who said i had any, i was just enquiring for a friend of mine :LolLolLolLol:
i know your lying jim you got no mates
-
i've been rumbled.